Boiler steel plate P265GH is produced according to standard EN 10028-2. Boiler steel plate P265GH owns the minimum yield strength of 265 Mpa. Therefore, plate P265GH can be used in higher strength situiations for boilers and tanks. Boiler steel plate P265GH needs to be done normalizing treatment.
Boiler steel plate P265GH chemical composition:
Maximum percentage of Carbon (C): 0.20.
Maximum percentage of Manganese (Mn): 0.80 and minimum percentage: 0.40
Maximum percentage of Phosphorous (P): 0.025
Maximum percentage of Sulphur (S): 0.015
Maximum percentage of Chromium: 0.30
Maximum percentage of Nickel (Ni): 0.30
Maximum percentage of Silicon (Si): 0.40
Maximum percentage of Molybdenum (Mo): 0.08
Maximum percentage of Nitrogen (N): 2.0 and minimum: 0.01
Maximum percentage of Copper (Cu): 0.30
Maximum percentage of Titanium (Ti): 0.03
Maximum percentage of Niobium (Nb): 0.02
Minimum percentage of Aluminum (Al): 0.02
Maximum percentage of Vanadium (V): 0.02
The boiler steel plate P265GH chemical composition is close to that of ASTM A516 grade 60 steel. The ASTM A516 grade 60 steel is P265GH steel equivalent grade in ASTM standard. BBN steel is world class boiler steel plate supplier. For any information about boiler steel plate P265GH, such as boiler steel plate P265GH chemical composition, plate P265GH mechanical property, boiler steel plate P265GH specification, boiler steel P265GH data sheet, plate P265GH price, please feel free to consult BBN steel.