Under EN 10025-2,there are three different steel grade for S275,it is S275J2,S275J0 and S275JR.S275j2 steel plate need to be done low temperature impacting test under minus 20 centigree,S275J0 done under zero centigree and S275JR steel plate done this impacting test under room temperature.
Thickness (mm)
|
|||||||||
S275J2
|
≤ 16
|
> 16 ≤ 40
|
> 40 ≤ 63
|
> 63 ≤ 80
|
> 80 ≤ 100
|
> 100 ≤ 150
|
> 150 ≤ 200
|
> 200 ≤ 250
|
> 250
|
Yield strength (≥Mpa)
|
275
|
265
|
255
|
245
|
235
|
225
|
215
|
205
|
195
|
|
< 3
|
≥ 3 ≤ 100
|
> 100 ≤ 150
|
> 150 ≤ 250
|
> 250
|
||||
Tensile strength (Mpa)
|
430-580
|
410-560
|
400-540
|
380-540
|
380-540
|
Main chemical elements composition of S275J2
|
|||||||
Thickness(mm)
|
C
|
Si
|
Mn
|
P
|
S
|
N
|
Cu
|
T≤16
|
0.18
|
...
|
1.50
|
0.025
|
0.025
|
...
|
0.55
|
16<T≤40
|
0.18
|
||||||
40<T
|
0.18
|