C
|
Si
|
Mn
|
Ni
|
P
|
S
|
Cr
|
Mo
|
max 0.22
|
max 0.45
|
0.85–1.75
|
max 0.55
|
max 0.035
|
max 0.030
|
max 0.35
|
max 0.13
|
V
|
Nb
|
Ti
|
|
|
|
|
|
max 0.14
|
max 0.06
|
max 0.06
|
|
|
|
|
|
Temperature
|
-20
|
-10
|
0
|
20
|
Notch impact test. Min. absorbed energy
|
40
|
43
|
47
|
55
|
Nominal thickness (mm)
|
to 16
|
16 - 40
|
40 - 63
|
63 - 80
|
80 - 100
|
100 - 150
|
150 - 200
|
ReH - Minimum yield strength (MPa)
|
355
|
345
|
335
|
325
|
315
|
295
|
286
|
Nominal thickness (mm)
|
to 100
|
100 - 200
|
Rm -Tensile strength (MPa)
|
470-630
|
450-600
|
Nominal thickness (mm)
|
to 16
|
16 - 40
|
40 - 63
|
63 - 80
|
80 - 200
|
A - Minimum elongation Lo = 5,65 √ So (%)
|
22
|
22
|
22
|
21
|
21
|
Germany
DIN,WNr
|
France
AFNOR
|
England
BS
|
Italy
UNI
|
China
GB
|
Russia
GOST
|
StE355
|
E 355 R
|
|
Fe E 355 KG N
|
|